As Cast Finish |
End Finish or Use |
| 1. |
Surface imperfections (cold shut, blisters, oil flow marks, surface porosity, etc.) non objectionable. |
Surface finish of no importance |
| 2. |
Some Surface imperfections (Cold Shut, rubs, surface porocity etc.) not objectionable. |
Protective Coatings :
Anodize (non-decorative)
Chromate
Heavy paint
Matte or wrinkle finish |
| 3. |
Slight Surface imperfections (Cold Shut, rubs, surface porocity etc.) can be removed by spot polishing, not objectionable |
Decorative Coatings:
Lacuers
Enamels
Plating (AI)
Chemical Finish
Polished Finish |
| 4. |
Surface imperfections, that can be removed by automatic buffing only, not objectionable |
Structural parts (High stress areas)
Plating(Zn)
Electrostatic Painting |
| 5. |
No objectionale surface imperfectiones that would be highlighted by eletctro-chemical polishing. Where surface waviness (Flatness) noted by light reflection is a reason for rejection. Special agreement should be reached with the die caster |
|